Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX630 - Europe - (PPE+PP)-GF30 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX630 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL PPX™ 630 resin is a 30% glass reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high elongation and high stiffness along with temperature performance, impact resistance, hydrolytic and dimensional stability. NORYL PPX630 resin is an excellent candidate for hot water system exteriors, condensate housings, and printer internals. *See NORYL PPX630F resin for NSF 61.

UL Yellow Card Link E45329-100962693
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 3 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 6600 MPa ISO 527
Stress at break 80 MPa ISO 527
Strain at break 4.1 % ISO 527
Flexural modulus 5500 MPa ISO 178
Charpy impact strength, +23°C 50 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 50 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 15 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 48 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 46 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, 4mm 15 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 10 kJ/m² ISO 180/1A
Ball indentation hardness 75 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, B 125 °C ISO 306
Vicat softening temperature, 120°C/h 50N 128 °C ISO 306
Coeff. of linear therm. expansion, parallel 20 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 115 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.4 - IEC 62631-2-1
Dissipation factor, 1MHz 10 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Comparative tracking index 500 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.2 % Sim. to ISO 62
Density 1190 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 260 - 300 °C -
Mold temperature 40 - 65 °C -
Feed temperature 60 - 80 °C -
Zone 1 245 - 290 °C -
Zone 2 250 - 290 °C -
Zone 3 255 - 290 °C -
Characteristics
Processing
Injection Molding
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.